TriStar II Plus – How to Run a Nitrogen BET Surface Area Analysis w/ Carbon Black Reference Material

This video will show how to run a nitrogen BET surface area analysis with carbon black reference material on the Micromeritics TriStar II Plus Surface Area and Porosity Analyzer.
AutoChem II – Injection Loop Replacement

This video will walk you through how to change the injection loop on a Micromeritics AutoChem II Automated Catalyst Characterization System.
Autochem II – Sample Preparation for Chemisorption Analyses

This video will show you how to prepare and load the sample tube for the chemisorption analyses on the Micromeritics AutoChem II Automated Catalyst Characterization System.
AutoChem II – TCD Calibration

This video will show you how to perform a TCD calibration on the Micromeritics AutoChem II Automated Catalyst Characterization System. Remember to always consult your operator’s manual for more detailed information.
AutoChem II – Carbon Monoxide Pulse Chemisorption Analysis with Platinum Alumina (PtAl)

This video will show how to run a Carbon Monoxide pulse chemisorption analysis with the platinum alumina (PtAl) reference material on the Micromeritics AutoChem II Automated Catalyst Characterization System.
AutoChem II – Microactive Software – Peak Editor for Temperature Programmed Reduction (TPR)

This video will show you how to use the Peak Editor for a Temperature Programmed Reduction on the Autochem II Microactive Software.
AutoChem II Microactive Software – Peak Editor Pulse Chemisorption

This video will show you how to use the Peak Editor for Pulse Chemisorption on the AutoChem II Microactive Software.
Autochem II – How to Run a Temperature Programmed Reduction (TPR) with a Silver Oxide Reference Material

This video will show you how to run a Temperature Programmed Reduction (TPR) with silver oxide reference material on the Micromeritics AutoChem II Automated Catalyst Characterization System.
3Flex – Sample Preparation for Physisorption Analyses

This video will show you how to prepare and load the sample tube for the physisorption analyses on the Micromeritics 3Flex Surface Characterization Analyzer.
3Flex – Vapor Purification

This video will show how to assemble the vapor source on the Micromeritics 3Flex Surface Characterization Analyzer.